Sagging

Excessive flow on vertical surface resulting in drips on the painted surface.

The Causes

  • Improper spray gun setting
  • Thin paint viscosity
  • Short flash-off time when painting

  • Thick paint application

How to Fix

  1. Prepare low-grit sandpaper to condition area
  2. Sand, clean, & polish defective areas with Nippon Paint 910 Speed-Cut Compound or Nippon Paint 920 Ultra-Cut Compound